中国化工网首页 >> 化工助手 >> 化学配方数据库
配方类型: |
METALS AND THEIR TREATMENT |
配方说明: |
Lighter Flint Alloy (Pyrophoric) |
配制方法: |
Mischmetal with 12 to 17% zinc is extruded at 380 to 400'C. at 4100 to 4800 kg. per sq.in. The pyrophoric properties are improved by the addition of 2 to 4% cadmium and 1.5% copper. The alloy is chill cast at 100 to 500'C. |
|