配方类型: |
COSMETICS |
配方说明: |
Shaving Gel Containing Water Soluble Lubricant |
配方组成: |
Isopentane/6.00 Palmitic Acid/6.00 Germaben II/1.00 Fragrance and Dye/q.s. Polyox WSR-205/0.10 Water/73.42 Triethanolamine, 99%/5.00 Ameroxol OE-20/2.00 Water/3.23 Cellosize Polymer PCG-10/1.25 Glycerin/2.00 |
配制方法: |
Add Cellosize to water at room temperature with rapid stirring. When well dispersed, heat to 75'C. Make a 3.00% solution using 0.10 g to Polyox WSR-205 to 3.23 g water. Add to Cellosize dispersion as it is heating to 75'C. When batch is at 75'C and a clear gel has formed, add palmitic acid, triethanolamine, Ameroxol OE-20, glycerin and Germaben II to batch, individually, waiting for each ingredient to dissolve before adding the next one. When batch is uniform, cool to room temperature and add fragrance and dye. Allow air to escape from the mixture. Cool Isopentane and shave gel to 15'C. Add Isopentane slowly to batch with gentle stirring to avoid introducing bubbles or foam. Package in seprotype aerosol cans with A-46 propellant. |
|