中国化工网首页 >> 化工助手 >> 化学配方数据库
配方类型: |
ADHESIVES |
配方说明: |
Corrugating Starch (Upper Mixer) |
配制方法: |
Add cold water to 23.75 in. from top. Heat to 130'F. and add 180 lb. corrugating starch. Mix 10 minutes, then add 34 lb. caustic soda in 4 gal. water and mix 15 minutes. Cook with live steam to 165'F. and then add water to 6 in. from top. |
|