配方类型: |
METALS AND THEIR TREATMENT |
配方说明: |
Foundry Sand Core and Mold (U.S. Patent 2,765,507) |
配方组成: |
Kerosene/0.25-0.75 Water-Soluble Polyacrylic Acid/0.3-1 High Grade Foundry Sand/To make 100 Moisture/2.5-5 |
配制方法: |
Mold and air-oven dry at 200 to 350'F. for 10 to 30 minutes. This gives a high hot strength core or mold. |
|