    配方类型: PAPER
    配方说明: Paper-Coating Adhesive
    配方组成: Soda Ash/3
    Borax/15
    Dry Casein/100
    配制方法: Prepare the adhesive solution as heavy as possible and dilute to the proper strength just before using.
    Stir the adhesive solution in a heavy concentration at the preparation temperature for 1 to 2 hours to impart increased elasticity. Also stir until cold to prevent the forming of any scum on the top of the adhesive solution. The casein solution may be used "hot" or "cold" according to the practice of the individual operator. Time and choice of quantity of alkali to be used in the preparation of the casein adhesive will also vary with the individual mill as seen in formulae 1 to 18.
    Ammonia, because of its volatility and cost, is frequently added at the end of the operation.
    The order of addition of soda ash is governed by the presence of free acid in the casein. Excess acidity will result in foaming. Satisfactory results have been obtained with the following sequence: a Borax, soda ash, and ammonia b Caustic soda, sodium fluoride, and soda ash While the usual temperatures of 110 to 130'F., or

    返回数据库查询
    其他库:化学品法规 国家标准 化学品安全数据库(msds) 外贸常识 合同范本 报关指南 商检指南 国际区号 国家代码