配方类型: |
RUBBER, RESINS, PLASTICS AND WAXES |
配方说明: |
Cation-Exchange Resin (Indian Patnet 47,468) |
配方组成: |
Formaldehyde/110 cc. Naphthalene/52 g. Sulfuric Acid (66'Be.)/33 cc. |
配制方法: |
Heat the naphthalene to 120'C. and add the acid, with stirring. Then heat at 140 to 150'C. for 5 to 6 hours. Cool to 90'C. and add the formaldehyde, with good stirring, until a hard black resin results. Wash with water and regenerate with 5% hydrochloric acid. |
|