    配方类型: INKS
    配方说明: Flexographic White Ink for Paper, Polyethylene, Etc.
    配方组成: White shellac/27
    Titanium dioxide, rutile/40
    Denatured alcohol, anhydrous/33
    charge into pebble mill and allow to mill for 16 hours. Shellac must
    be fresh; it may be pre-dissolved in alcohol before charging mill, if
    desired.
    If a single batch is to be made, hold out 5 parts of the specified
    amount of alcohol, using this as a mill post-wash, to be added to the
    major portion of the ground ink, drained from the mill before the wash
    is charged.
    Thin with denatured alcohol at press as needed (approx. 20%).
    Polyethylene must have high treatment level.
    Formula No.
    Titanium dioxide/33
    Resin (polyamide)/26
    Isopropanol/41