配方类型: |
RUBBER, PLASTICS, WAXES |
配方说明: |
Reinforcing Polyol Improves Strength at Low Density |
配方组成: |
$G: "Pluracol" PEP-450 Within the effective proportions, incorporation of "Quadrol" improves cell structure, content of closed cells, and retention of "K" factor. The formulation with 80 to 20 ratio provides foam that is technically and economically practical "Dow Corning" 113/3.0 Triethylamine/1.0 Tetramethylguanidine/2.5 "Quadrol" Fluorocarbon 11/65.0 $G: "Niax" Triol LK-380 "Quadrol" "PAPI" Rise time (min-sec) Core Density (pcf) Compressive strength (core parallel to rise) psi at 2.5% deflection "PAPI" "Dow Corning" 113/3.0 Rise time (min-sec) Core density (pcf) Compressive strength (core parallel to rise) psi at 2.5% deflection b: "Pluracol" PEP-450/As shown Triethylamine/1.0 a: "PAPI"/As shown a: "PAPI"/As shown fluorocarbon 11/45.0 Tetramethylguanidine/3.0 b: "Niax" Triol LK-380/As shown "Quadrol"/As shown "Quadrol"/As shown |
配制方法: |
To obtain maximum strength in low-density foams, it is desirable to use a dry resin with the minimum hydroxyl functionality of three. With resins that do not fit in this category, useful foams can be obtained by adding a reinforcing resin such as "Quadrol." |
|