配方类型: |
RUBBER, PLASTICS, WAXES |
配方说明: |
Polyester Resins |
配方组成: |
Methyl Ethyl Ketone Peroxide/1 Coat the surface of articles, e.g., brick, stone, paper, wood, etc., and bake at 150'F for 10 minutes, followed by 300'F for 5 minutes. Formula No.4 (Room-Temperature Coating "Synvar" V-50/100 Benzoyl Peroxide/2 "MR"-28C Resin/100 "MC"-1 Paste Catalyst/3 Accelerator E/2 "Bakelite" QRS-179/100 "Paraplex" P-43/75.0 "Paraplex" P-13/25.0 "Lupersol" DDM/1.0 Cobalt Naphthenate/1.6 |
配制方法: |
Spray, dip, or paint the surface and allow it to cure. |
|