| 配方类型: |
METALS |
| 配方说明: |
Flux for Lead Burning (U.S. Patent 2,596,466) |
| 配方组成: |
Ammonium Bromide/3 Stannous Chloride/2 Ammonium Acid Fluoride/1 Ammonium Hydroxide/23 Silver Chloride/1 Zinc Chloride/60 Water/10 |
| 配制方法: |
This mixture is heated at 180 to 200'F, cooled at 100 to 120'F, and water is then added to suit. |
|