| 配方类型: |
METALS |
| 配方说明: |
To Seal Porous Light Metal Castings (U.S. Patent 2,680,081) |
| 配方组成: |
Water/To make 100 cc Chromic Acid/7 g Potassium Dichromate/5 g Waterglass/50 cc |
| 配制方法: |
The castings are placed in a vacuum and then in the solution at 95 to 100'C for half an hour at 60 to 80 lb/sq inch pressure. |
|