中国化工网首页 >> 化工助手 >> 化学配方数据库
配方类型: |
PAPER |
配方说明: |
Paper Coating |
配方组成: |
Glyoxal/0.48 Latex/8.00 Water as needed for a solids content of 555 to 60% No. 11 Roll Coater (For Letterpress Paper Preservative/- *the casein should be cooked for 45 min at 55'C in the presence of 14% aqueous ammonia (based on dry casein). the casein solution should then be slowly added to the pigment dispersion. Clay (predispersed)/100.0 Butadiene-styrene latex/18.0 Dispersant/0.1 "Vinol" 125 polyvinyl alcohol/3.0 "Virset" A-130/0.5 Surfynol PC defoamer/0.1 Lubricant (solids)/1.0 "Aircoflex" 100 (solids)/16.0 LV protein, NH4OH cut/- Clay (predispersed)/90.0 Titanium dioxide/10.0 Dispersant/0.1 CaCO3, precipitated/35.00 "Vinol" 125 polyvinyl alcohol/5.0 "Virset" A-130/1.0 Enzyme converted starch/- "Surfynol" PC defoamer/0.1 Lubricant (solids)/1.0 "Aircoflex" 100 (solids)/10.0 T.S.P.P../- Clay (predispersed)/90.0 Preservative/- Titanium dioxide/10.0 Dispe |
配制方法: |
Water as needed for a solids content of 55% to 60%. |
|